Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 191 °C | 376 °F | DSC |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Melting Point | 191 - 202 °C | 375 - 395 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 15N95UV is a polyether copolymer-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis resist.. |
|||
Melting Point | 191 - 201 °C | 376 - 394 °F | |
UBE 5033B Air Blown Nylon 6/66 Film Specialties: Standard nylon 6/66Medium shrink, Low slipApplications: Best for Middle layer usageProcessing: Top web (Air blown)Thermoforming (T-die)Information provided by UBE. |
|||
Melting Point | 191 - 201 °C | 376 - 394 °F | |
UBE 5033FDX27 Air Blown Nylon 6/66 Film Specialties: High slip typeMedium shrinkApplications: General purposeSuitable for Water cooling processProcessing: Sausage casings (Water)Big bag (Air blown)Information provided by UBE. |
|||
Melting Point | 191 °C | 376 °F | ASTM D3418 |
Ashley Polymers Ashlene® L935 Nylon 11 An economy grade, unplasticized Nylon 11 for extrusion applications. Also available is L935H, same with UV and heat stabilizer.Data provided by the manufacturer |