Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 183 °C | 361 °F | |
Omnia Plastica PA 11 Rilsan B The only engineering plastic of natural origin (derived from castor oil), it is a polyamide which, unlike the other nylons, does not absorb humidity. It has all the good mechanical features of polya.. |
|||
Melting Point | 183 °C | 361 °F | DSC, both heating and cooling speeds of 10°C/min |
Noltex Soarnol® DC3203F Ethylene Vinyl Alcohol Copolymer Low ethylene content. Suitable for use in packaging material used at normal temperature and humidity. Ethylene content 32 mol%. Volatile matter 0.3%.Information provided by Soarus, LLC. In the Un.. |
|||
Melting Point | 183 °C | 361 °F | DSC |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Melting Point | 183 °C | 361 °F | DSC |
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat.. |
|||
Melting Point | 183 - 200 °C | 361 - 392 °F | |
Indium Corp. Indalloy 113 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 268 °C | 361 - 514 °F | |
Indium Corp. Indalloy 145 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 °C | 361 °F | Eutectic |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 183 °C | 361 °F | |
Lucas-Milhaupt 63 Sn-37 Pb Tin/ Silver Solder Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is desired. This allo.. |
|||
Melting Point | 183 - 192 °C | 361 - 378 °F | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 199 °C | 361 - 390 °F | |
Indium Corp. Indalloy 112 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 205 °C | 361 - 401 °F | |
Indium Corp. Indalloy 114 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 218 °C | 361 - 424 °F | |
Indium Corp. Indalloy 120 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 222 °C | 361 - 432 °F | |
Indium Corp. Indalloy 122 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 183 - 216 °C | 361 - 421 °F | |
Johnson Matthey JM5050 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 183 - 188 °C | 361 - 370 °F | |
Williams Advanced Alloys WS188 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 - 212 °C | 361 - 414 °F | |
Williams Advanced Alloys WS212 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 - 288 °C | 361 - 550 °F | |
Williams Advanced Alloys WS288 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 183 °C | 361 °F | |
Goodfellow Tin 60/Lead 39/Antimony 1 Alloy A general purpose, low melting point soft solder which can also be used as a protective coating and for metal film capacitors.Information provided by Goodfellow. |
|||
Melting Point | 183 °C | 361 °F | DIN 53 736 |
Hippe PA 11 Nylon 11 Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESHV Nylon 11, Blow Molding Grade (Dry) Designation ISO 1874-PA11,E,24-010Rigid grade for extrusion blow molding. Available color: natural. Additive free.Very good impact strength. Well adapted melt strength. High chemical resistance.Food.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry) Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good .. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMN D Nylon 11 (Dry) Designation ISO 1874-PA11,MR,12-010Rigid grade for injection molding. Available colors: black, blue, natural, orange, white. Mold release agent.High mechanical properties. Easy filling of the mold d.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMN Y TLD Nylon 11, MoS2 Filled (Dry) Designation ISO 1874-PA11,MHLR,12-020,MD05Rigid grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold release agent.No need of lubricant. L.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BMV Nylon 11 (Dry) Designation ISO 1874-PA11,M,18-010Rigid grade for injection molding. Available color: natural. Free additive.High impact strength. Easy filling of the mold due to its well adapted melt viscosity. Lo.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BZM 43 G9 Nylon 11, 43% Glass Fiber Filled (Dry) Designation ISO 1874-PA11,MS,18-080,(G+C)(F+D)(45+05)Rigid grade with glass fiber (43%) and graphite filler for injection molding. Available color: steel black gray. Additive free.High rigidity. Hig.. |
|||
Melting Point | 183 °C | 361 °F | (Dry) |
Arkema Group Rilsan® BESN P20 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-004Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.Flexibility. High impact strength. Very good chemical resistan.. |
|||
Melting Point | 183 °C | 361 °F | 10°C/min |
Arkema Group Rilsan® BESVO A FDA Nylon 11 (Dry) Designation ISO 1874-PA11,E,22-010Rigid grade for tubes and films extrusion in food applications. Available color: natural. Additive free.Good thermal and chemical resistance. Transparency. Barrier .. |
|||
Melting Point | 183 - 190 °C | 361 - 374 °F | |
Johnson Matthey JM6040 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 183 °C | 361 °F | DSC |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |