Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1760 °C | 3200 °F | |
Pyrotek Valcor® G-AZ Pre-Cast Shapes ApplicationsBurner blocks Skimmer blocks Cover blocks Specialty blocks Plungers Stirrers Spouts Feeder tubes AdvantagesProven performance in molten glass contact applications Smooth surface finish d.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® 6001-M-5 Kaolin Bulk Fiber Fiberfrax Bulk Fibers are manufactured to be used as feedstock in manufacturing processes or other applications where product consistency is critical. Manufactured on large, computer-controlled fur.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® HS70C High Purity High-Index Fiber In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® HSA-HP High Purity High-Index Fiber In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® Long Staple Fine AZS Large-Diameter Fiber In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® Long Staple Medium AZS Large-Diameter Fiber In addition to Fiberfrax Bulk Fibers, Unifrax has the ability to produce many different specialty fibers that provide a variety of desirable performance properties for certain applications. These f.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Foamfrax® Grade I Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Foamfrax® Grade II Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durabl.. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® Duraboard® HD Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® Duraboard® LD Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |
|||
Melting Point | 1760 °C | 3200 °F | |
Zircar Ceramics ASBF-1 Alumina-Silica Bulk Fiber Type ASBF-1 Alumina-Silica Bulk Fiber is a specially processed fiber which has low shot content and relatively short fiber length. Suitable for vacuum forming of rigid boards & shapes in a range of .. |
|||
Melting Point | 1760 °C | 3200 °F | |
Unifrax Fiberfrax® Duraboard® RG Ceramic Fiber Board Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard .. |