Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 172 °C | 342 °F | Crystallinity by DSC; ASTM D 3418 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Melting Point | 172 °C | 342 °F | DSC |
Lubrizol Estane® ZHF 90AT0 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 90AT0 TPU is a clear, glossy, zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding TPU properties.Uses: Cable jacket and tube/hos.. |
|||
Melting Point | 172 °C | 342 °F | ASTM D3418 |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Melting Point | 172 °C | 342 °F | |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Melting Point | 172 °C | 342 °F | By DSC |
Toyobo PELPRENE™ P40H Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melting Point | 172 °C | 342 °F | By DSC |
Toyobo PELPRENE™ P40H-05 Polyester TPE, Non-smell, Non-deposit Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo. |
|||
Melting Point | 172 °C | 342 °F | By DSC |
Toyobo PELPRENE™ P40U Polyester TPE, Weather-resistant Features: Polyester TPE, Weather-resistantInformation provided by Toyobo. |
|||
Melting Point | 172 °C | 342 °F | DSC |
Lubrizol ESTANE® ETE60DS3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, high transparencyUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket; Injection molding: VariousAvailable in.. |
|||
Melting Point | 172 °C | 342 °F | ASTM D3418 |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Melting Point | <= 172 °C | <= 342 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 00623 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00623 is a good coextrusion partner in extrusion coating, blown and cast film. Excellent sealing material with a very low seal initiation temperature. Availability: Africa & .. |
|||
Melting Point | <= 172 °C | <= 342 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 7511 is a very high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt ad.. |
|||
Melting Point | 172 °C | 342 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® XG5855 TPC-ET Extrusion Grade |
|||
Melting Point | 172 °C | 342 °F | ASTM D3448 |
Ensinger TECAFLON™ PVDF Polyvinylidene Fluoride (PVDF) - extruded products Polyvinylidene fluoride, or PVDF, is a fluorinated thermoplastic resin which has good resistance to most mineral and organic acids, aliphatic and aromatic hydrocarbons, alcohols, halogenated solvent.. |
|||
Melting Point | 172 °C | 342 °F | ASTM D3418 |
Arkema Group Pebax® 7033 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Melting Point | 172 °C | 342 °F | ISO 11357 |
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Melting Point | 172 °C | 342 °F | ISO 11357 |
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Melting Point | 172 °C | 342 °F | (Dry) |
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Melting Point | 172 °C | 342 °F | 10°C/min |
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Melting Point | 172 °C | 342 °F | ISO 11357 |
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Melting Point | 172 °C | 342 °F | ASTM D789 |
Arkema Group PLATAMID® 8020 Copolyamide Platamid® 8020 is a transparent, thermoplastic copolyamide designed for conversion by standard molding or extrusion techniques.Information provided by Arkema Group |