Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 165 °C | 329 °F | Masterbatch; ISO 11357-1,-3 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 3.2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1631 Bicomponent Polyester/PET Fiber Type - 4 Denier X 2 Inches Semi-crystalline low melt polyester sheath/PET core. Luster: Semi-Dull. Finish: HydrophilicApplications of bicomponent polyester fiber: Absorbent products, FDA-compliant products, non-wovens, fi.. |
|||
Melting Point | 165 °C | 329 °F | ISO 11357 |
Polyram RamOfin PPC101 Polypropylene Copolymer, Heat Stabilized Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamTal PM7002 Acetal, UV Stabilized UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamTal RM7009 Acetal, UV Stabilized UV stabilized acetal copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Total PPC 10641 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10641 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10641 is characterized by high fluidity with good mechanical prope.. |
|||
Melting Point | 165 °C | 329 °F | DSC |
Total PPH 3925WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect.. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Total PPH 4022 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4022 is a clarified nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4022 has been developed for extrusion-thermoforming, providing improved rigidity and impact r.. |
|||
Melting Point | 165 - 175 °C | 329 - 347 °F | ISO 11357 |
Polyram PlusTek PD502G6 Nylon 12 for Injection Molding, 30% Glass-fiber Reinforced 30% Glass-fiber reinforced, V-0 1.6 mm, Nylon 12 for injection molding application.Information provided by Polyram. |
|||
Melting Point | 165 °C | 329 °F | DSC |
Total PPH 3825 Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerEasy Flow - FINA 3825 exhibits exceptionally easy flow characteristics.FDA - FINA 3825 complies with all applicable FDA regulations for food contact applicatio.. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamOfin PPC501 Polypropylene, Flame Retardant Flame retardant polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamOfin PPH300G8 Polypropylene, 40% Glass Fiber 40% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamOfin PPH307G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Eurostar Starpylen M1000-BK1A987 PP, Carbon Black Starpylen M1000-BK1A987 is a high carbon black load PP resinInformation provided by Eurostar. |
|||
Melting Point | 165 °C | 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecoform® PO30 GR20 NL HS POM, 20% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 165 °C | 329 °F | ASTM D789 |
Aclo Accucomp Polyacetal (POM) ACE091L High Viscosity |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 555 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 380 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 520 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 °C | 329 °F | ISO 3146 |
Total PPC 10712 Polypropylene, Heterophasic Copolymer ATOFINA Propylene 10712 is a nucleated and controlled-rheology heterophasic copolymer. PPC 10712 is characterized by good stiffness and impact resistance as well as low shrinkage and low warpage. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram PM3013G2 Acetal, 10% Glass Fiber
(discontinued **) 10% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | |
Polyram RamTal PM1009 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melting Point | 165 °C | 329 °F | |
Tisan TISAKRIL® 30% Glass Fiber Reinforced ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |