Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1500 °C | 2730 °F | |
Unifrax Foamfrax® Isofoam Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Unifrax Isofrax® 1260C Paper Fiber Isofrax® 1260C Paper is a unique product which is manufactured by forming Isofrax 1260C Fiber in a nonwoven matrix. The fibers are randomly oriented during manufacture, then held in place with a l.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Goodfellow Chromaloy O® Resistance Alloy Resistance heating alloy with excellent resistance to oxidation at elevated temperatures. Used in many varied applications - from small household appliances to large industrial furnaces.Information .. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RS-200 Refractory Sheet ZRCI Refractory Sheet Type RS-200 is a fiber-reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Melting Point | >= 1500 °C | >= 2730 °F | |
Zircar Refractory Composites RSBL-SOL6 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Melting Point | >= 1500 °C | >= 2730 °F | |
Zircar Refractory Composites RSBL-SOL8 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RS-Cloth Refractory Sheet Refractory Sheet RS-Cloth is ceramic fiber reinforced alumina composite. It offers the strength, durability, flexibility and versatility required by many high temperature applications up to 1300°C(.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RS-MS ALUMINA MOLDABLE SLEEVING ZIRCAR Refractory Sheet Type RS-MS Moldable Sleeving is a moist woven alumina composite sleeving. It is supplied in a wet form ready for the fabrication of custom shapes. It can be cut to size with .. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RSPA-SOL3 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RSPA-SOL4 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RS-1200 Refractory Sheet ZIRCAR Refractory Sheet Type RS-1200 is a high strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 1300°C(2372°F). RS-12.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Zircar Refractory Composites RS-201 Refractory Sheet ZRCI Refractory Sheet Type RS-201 is a fiber reinforced ceramic laminate with useful properties to 1260°C (2300°F). This high temperature product offers high strength, moderate thermal conductivit.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
Melting Point | >= 1500 °C | >= 2730 °F | |
Johnson Matthey Amoxis 10-1R N2O Abatement Catalyst Odorless solid pellets, various dimensions. During the manufacture of Nitric Acid, significant quantities of pollutants are released into the atmosphere. One of the principal pollutants is the gree.. |
|||
Melting Point | 1500 °C | 2730 °F | |
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |