Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1454 °C | 2649 °F | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Melting Point | 1454 °C | 2649 °F | |
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum 420 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Melting Point | 1454 °C | 2649 °F | |
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Melting Point | 1454 °C | 2649 °F | |
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Melting Point | 1454 °C | 2649 °F | |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Melting Point | 1454 °C | 2649 °F | |
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Melting Point | 1454 °C | 2649 °F | |
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 288°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 538°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 649°C (1200°F) Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420HC Allegheny Ludlum Type 420HC is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainl.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Annealed Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 204°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 316°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 427°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |
|||
Melting Point | 1454 - 1510 °C | 2649 - 2750 °F | |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 420, Hardened + 482°C Temper Allegheny Ludlum Type 420 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |