Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1427 - 1454 °C | 2601 - 2649 °F | |
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip General Elgiloy® information: High strength, ductility, fatigue life, and good mechanical properties. Corrosion resistant in numerous environments. Available in strip (currently 0.0015" to 0.075".. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 20% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 50% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction The strength, elongation, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fati.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 85% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, Heat Treated Heat Treatment 5 hours at 482°C. The strength and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, duc.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Strip, 30% Cold Reduction, Heat Treated Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High .. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 10% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 20% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 40% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction The strength, shear modulus, and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, f.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 65% Cold Reduction, Heat Treated Heat Treatment 5 hours at 527°C. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: Hi.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Carpenter Invar 36® Alloy, Annealed Bars and Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Carpenter Invar 36® Alloy, Cold Drawn Bars Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Carpenter Invar 36® Alloy, Cold Rolled Strip Data provided by Carpenter Technology Corporation.Carpenter Invar "36" alloy is a 36% nickel-iron alloy possessing a rate of thermal expansion approx. one-tenth that of carbon steel up to 200°C. T.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Carpenter Glass Sealing "42-6" Alloy A nickel-chromium-iron which has been developed to match the thermal expansion characteristics of 0120 glass. An additional advantage of this alloy for glass-to-metals seals is the tight dark green.. |
|||
Melting Point | 1427 °C | 2601 °F | |
Elgiloy® Co-Cr-Ni Alloy, Wire The strength and hardness values are specific to this cold reduction treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High strength, ductility, fatigue life, and.. |