Thermal Properties Metric English Comments
Melting Point 1352 °C
2465 °F
Universal Wire Works No. 21 Cobalt Alloy Welding Wire
Universal No. 21 is a cobalt-chromium-molybdenum alloy designed for covered electrode, TIG, MIG, hard surfacing applications. The work-hardening characteristics, high ductility properties, excellent..
Melting Point <= 1352 °C
<= 2465 °F
Weartech International WT-800 Cobalt Hardfacing & Wear Resistant Alloy
Applications: Magnetic tape heads, valves, extruder barrelsInformation provided by Weartech International