Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® Green Polyethylene Material ”S”® is based on virgin, ultrahigh molecular weight low pressure polyethylene and significantly exceeds the requirements of DIN 16972. In particular, Material ”S”® green has excellen.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146 |
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial Material ”S”® plus + AB contains special substances that prevent the growth of bacteria and other microbes. The material is thus ideally suited for use when manufacturing and processing foods.Sp.. |
|||
Melting Point | 130 - 138 °C | 266 - 280 °F | ISO 3146 |
Polikim ULPOLEN® 1000 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, UV - stabilized OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | ISO 3146; DSC, 10°C/min |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Melting Point | 130 °C | 266 °F | ASTM D3418 |
ExxonMobil HD 6605.29 Injection Molding Resin
(discontinued **) HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for .. |
|||
Melting Point | 130 - 134 °C | 266 - 273 °F | ASTM D3418 |
Arkema Group Kynar Flex® 2950 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Melting Point | 130 - 145 °C | 266 - 293 °F | ISO 3146-C |
FKuR Kunststoff Terralene® LL 1303 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melting Point | 130 - 131 °C | 266 - 268 °F | Crystalline MP |
Garland Manufacturing GAR-DUR® Ultra High Molecular Weight Polyethylene (UHMW-PE) GAR-DUR® plastic parts are made from ultra high molecular weight (UHMW) polymer having a molecular weight of 4.2 million and greater. Garland Manufacturing Company has been processing UHMW resin .. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC H1501 Polypropylene Homopolymer Features: SEETEC H1501 is a homopolymer for injection molding. H1501 is specifically developed for application demanding a high stiffness and a high fluidity. SEETEC H1501 meets the FDA requirement .. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | Crystalline melting range |
Mikro-Technik Mikrolen UHMW-PE Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26.. |
|||
Melting Point | 130 - 173 °C | 266 - 343 °F | |
Indium Corp. Indalloy 101 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 130 - 140 °C | 266 - 284 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLBOND® 125/H Linear Thermoplastic Polyurethane Pearlbond™ 125H is polyester-based thermoplastic polyurethane, supplied in form of colourless, translucent granules, combining hardness with excellent low-temperature flexibility and a low soft.. |
|||
Melting Point | 130 - 136 °C | 266 - 277 °F | DSC |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Melting Point | 130 °C | 266 °F | |
Sanyo PELESTAT® 2450 Antistatic Additive PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) and give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a vari.. |
|||
Melting Point | 130 - 134 °C | 266 - 273 °F | ISO 3146 |
Borealis Borseal™ TD220BF Terpolymer for BOPP Film Borseal TD220BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD220B.. |
|||
Melting Point | 130 - 132 °C | 266 - 270 °F | crystalline; DSC |
Total Xsene® XS10 H HDPE, pipe, injection molding FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound.. |
|||
Melting Point | 130 °C | 266 °F | DSC |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,.. |
|||
Melting Point | 130 °C | 266 °F | Dow Method (DSC) |
Dow DMDA-8920 NT 7 High Density Polyethylene Resin DOW DMDA-8920 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Melting Point | 130 °C | 266 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6230 NT 7 High Density Polyethylene Resin (HDPE) Good extrusion characteristics Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6230 NT 7 is specifically designed for use in either intermittent or continuous blow molding equipment to.. |
|||
Melting Point | 130 °C | 266 °F | ASTM D3418 |
ExxonMobil HD 6605.70 Injection Molding Resin Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan.. |
|||
Melting Point | 130 - 138 °C | 266 - 280 °F | |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Melting Point | 130 - 138 °C | 266 - 280 °F | |
Arkema Group KYNAR® 2751-00 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasi.. |
|||
Melting Point | 130 - 135 °C | 266 - 275 °F | DSC ISO 3146 |
Okulen® 500 PE-HMW, Natural OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Melting Point | 130 - 136 °C | 266 - 277 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 130 - 132 °C | 266 - 270 °F | crystalline; DSC |
Total Xsene® XS10 Orange YCF HDPE, pipe FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance .. |
|||
Melting Point | 130 °C | 266 °F | |
Radici Radilene® R 70 IE 5058 B High Density Polyethylene Shore hardness: 64 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC R7700 Polypropylene, Random Copolymer Features: Seetec R7700 is designed for the extrusion of fibers with the spunbond technology. This grade is characterized by narrow MWD and good processability. SEETEC R7700 meets the FDA requirement.. |