Thermal Properties Metric English Comments
Melting Point 1250 - 1315 °C
2280 - 2399 °F
Reade Advanced Materials Garnet Powder (Fe3Al2(SiO4)3)
Description: A group of iron aluminum silicate homogeneous minerals having similar properties. Non-hygroscopic, sharp angular shape, inert, slightly magnetic, not soluble in water, translucent, fria..