Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1220 - 1270 °C | 2230 - 2320 °F | |
Special Metals FERRY® Alloy A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy .. |
|||
Melting Point | 1220 - 1390 °C | 2230 - 2530 °F | |
Special Metals UDIMET® alloy D-979 Fe-Ni Alloy UDIMET® alloy D-979 (UNS N09979) is an iron-nickel alloy designed for turbine disc applications at temperatures up to 1200-1400°F (649-760°C). Hardened by a complex precipitation of interm.. |