Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FF 33 Low Density Polyethylene - Blown Film Extrusion Riblene FF 33 is a high molecular weight low density polyethylene (LDPE), with added slip agent, ideal for blown film extrusion. Riblene FF 33 is characterized by a good melt strength leading to a .. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FF 34 Low Density Polyethylene - Blown Film Extrusion Riblene FF 34 is a high molecular weight low density polyethylene (LDPE), with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FF 34 is characterized by a good melt s.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FF 39 Low Density Polyethylene - Blown Film Extrusion Riblene FF 39 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 39 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FL 23 Low Density Polyethylene - Blown Film Extrusion Riblene FL 23 is a low density polyethylene (LDPE) with added slip agent, suitable for blown film extrusion. Riblene FL 23 is characterized by a good balance between processability and mechanical p.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FL 30 Low Density Polyethylene - Blown Film Extrusion Riblene FL 30 is a low density polyethylene (LDPE) ideal for blown film extrusion. Riblene FL 30 is characterized by a good balance between processability, mechanical and optical properties.Films m.. |
|||
Melting Point | 114 °C | 237 °F | Internal method |
Polimeri Europa Riblene® FM 34 E Low Density Polyethylene - Blown Film Extrusion Riblene FM 34 E is a low density polyethylene (LDPE) with added slip (erucamide) and antiblocking agents, suitable for blown film extrusion. Riblene FM 34 E is characterized by a good balance betwe.. |
|||
Melting Point | 114 °C | 237 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 3518 GA Premium Cast Film Resin
(discontinued **) Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Melting Point | 114 °C | 238 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 117.08 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3020 F LDPE Blown film, injection moldings, blow moldings.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3020 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3024 H LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3025 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3032 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3220 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3226 K LDPE, Film Grade FilmData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
LyondellBasell Lupolen® 3412 D LDPE Telephone cable insulationData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 114 °C | 237 °F | |
Hybrid Plastics POSS® MA0702 MethacrylIsobutyl-POSS® POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®.. |
|||
Melting Point | 114 °C | 237 °F | ISO 11357-3 |
Total FE 8000 LDPE blown film Low density radical polyethylene made by high pressure autoclave. Advised temperature profile : 160 to 200°C.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired form.. |
|||
Melting Point | 114 °C | 237 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 4518PA Premium Cast Film Resin Exceed 4518PA resin is a hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 4518PA resin have outstanding tensile properties and impact and puncture toughness.. |
|||
Melting Point | 114 °C | 237 °F | Freezing Point; ASTM D3418 |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Melting Point | 114 °C | 237 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® E528 Polymer Modifier DuPont™ Fusabond® E528 is a anhydride modified polyethylene. Used as a polymer modifier |
|||
Melting Point | 114 °C | 237 °F | Dow Method (DSC) |
Dow FLEXOMER™ DFDA-1095 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1095 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |
|||
Melting Point | 114 °C | 237 °F | Dow Method (DSC) |
Dow FLEXOMER™ DFDB-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDB-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |
|||
Melting Point | 114 °C | 237 °F | Dow Method (DSC) |
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |
|||
Melting Point | 114 °C | 237 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Melting Point | 114 °C | 237 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus R301B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R301B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Melting Point | 114 °C | 237 °F | ASTM D3418 |
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,.. |
|||
Melting Point | 114 °C | 237 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil Exceed™ 3518 CB Premium Cast Film Resin Exceed 3518 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 3518 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Melting Point | 114 °C | 237 °F | ISO 11357-3 |
Total Lacqtene® 1025 FH 24 LDPE blown film