Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1110 - 1190 °C | 2030 - 2170 °F | |
Wieland 1907 Wilaform Gold Palladium white gold alloy with beautiful grey-white color.Applications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Melting Point | 1110 - 1165 °C | 2030 - 2129 °F | |
Wieland 1916 Wilaform Gold Hard palladium white gold alloy with beautiful grey color.Applications: casting, chains, laminar decoration, pipes, tubingDental |