Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 110 °C | 230 °F | Internal method |
Polimeri Europa Riblene® MM 20 R Low Density Polyethylene - Injection Molding Riblene MM 20 R is a medium fluidity low density polyethylene resin (LDPE).Parts made by Riblene MM 20 R are characterized by a high flexibility.Main Applications: Riblene MM 20 R is suitable for i.. |
|||
Melting Point | 110 °C | 230 °F | ASTM D3418 |
Petroquimica Triunfo Trithene® JX 7065 LDPE - Injection Molding and Master Batch The Trithene® JX 7065 resin is a low-density polyethylene with a wide molecular weight distribution, developed to offer good impact resistance, excellent flexibility, and high resistance to stress .. |
|||
Melting Point | 110 - 200 °C | 230 - 392 °F | Average value: 151 °C Grade Count:29 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 641.LN Molding, Extrusion and Compounding Resin
(discontinued **) LD 641.LN is a low density homopolymer specifically designed for high performance blow molding applications. This resin is suitable for applications requiring high melt strength, flexibility, good .. |
|||
Melting Point | 110 °C | 230 °F | ASTM D3418 |
LyondellBasell Microthene® F FN51000 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 110 °C | 230 °F | ASTM D3418 |
LyondellBasell Microthene® F FN51900 Low Density Polyethylene General DescriptionMicrothene F polyolefin powders are ultra-fine, spherically shaped particles with narrow size distribution suitable for use in a broad range of specialty applications. Microthene.. |
|||
Melting Point | 110 - 130 °C | 230 - 266 °F | 0.025" extruded film, |
Huntsman IROGRAN® PS455-200 TPU-Polyester Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers.. |
|||
Melting Point | 110 °C | 230 °F | DSC |
LG Chemical LUTENE FB0300 LDPE Blown Film Grade Description: LUTENE FB0300 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of heavy duty sacks and pallet shrink films. LUTENE FB0300 have the e.. |
|||
Melting Point | 110 - 130 °C | 230 - 266 °F | |
LG Chemical LUTENE XL2700BK PE Compound Description: LUTENE XL2700BK has excellent strippability, processability, weather resistance, heat resistance for medium and high voltage power cables. The advantage of LUTENE XL2700BK over conventi.. |
|||
Melting Point | 110 °C | 230 °F | DSC |
LG Chemical LUTENE FB0800 LDPE Blown Film Description: LUTENE FB0800 is mainly intended for the extrusion of blown film with high mechanical property for the manufacture of greenhouse film. LUTENE FB0800 have the excellent mechanical proper.. |
|||
Melting Point | 110 °C | 230 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation .. |
|||
Melting Point | 110 - 155 °C | 230 - 311 °F | ISO 3146 |
Borealis Steripeel™ WD170CF PO Compound for Sterilizable Peelable Film Applications Steripeel WD170CF is a non-formulated film resin, specially developed for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WD170CF is suitable for various peelable.. |
|||
Melting Point | 110 °C | 230 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 4125 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
EMS-Griltech Griltex® D 1694A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 110 °C | 230 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LD 102.LC Thin Gauged Film Resin L Product Description: LD 102.LC is a formulated homopolymer, garment film resin with good toughness. It is capable of being drawndown to thing gauges.Availability: Latin America, North America and .. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | Sheath |
EMS-Griltech Grilon® BA 115 White Nylon 6/CoPA Bi-Component Fiber Description: GRILON BA 115 is the new core / sheath bi-component fiber based on PA 6/CoPA with a sheath melting range from 110 - 120 °C. The fine count bi-component fiber guarantees an even distrib.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® 1200 F Blend Biodegradable Polyester Description: A flexible plastic designed for film extrusion and extrusion coating. Ecoflex® F Blend 1200 comes closer than any other biodegradable plastic to the processing properties of LDPE and L.. |
|||
Melting Point | 110 - 115 °C | 230 - 239 °F | |
BASF N,N’-Dimethylolurea Formula: C3H8O2N3CAS: 140-95-4Description: N,N’-Dimethylolurea is a free flowing, white powder. It is readily soluble in hot water. Synonyms: DMOUApplications: Intermediate used in the production .. |
|||
Melting Point | 110 - 126 °C | 230 - 259 °F | |
3M Dyneon™ FX 5912 Dynamar™ Polymer Processing Additive Dynamar FX 5912 is a free-flowing fluorothermoplastic processing aid that is designed for use at very low levels to improve the processing of thermoplastics. Typical use levels of 200 to 1000 ppm ha.. |
|||
Melting Point | 110 - 122 °C | 230 - 252 °F | Average value: 115 °C Grade Count:10 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Melting Point | 110 °C | 230 °F | DSC |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® C1200 F Blend Biodegradable Polyester Description: Ecovio® F Blend C2332 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephathalic acid in the polymer chain. E.. |
|||
Melting Point | 110 - 120 °C | 230 - 248 °F | DSC |
BASF Ecoflex® P BX 7020 Biodegradable Polyester Description: Ecoflex® P BX 7020 is our biodegradable, statistical, aliphatic-aromatic copolyester based on the monomers 1,4-butanediol, adipic acid and terephthalic acid or dimethyltherephthalate i.. |