Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 163 - 173 °C | 325 - 343 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 091 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 163 - 173 °C | 325 - 343 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 091 WUF 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |