Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 115 - 125 °C | 239 - 257 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 820 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 115 - 125 °C | 239 - 257 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 820 SL 40 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 115 - 125 °C | 239 - 257 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 820 SLU 40 Unexpanded microspheres in aqueous dispersion Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 115 - 125 °C | 239 - 257 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 820 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |