Polymer Property : Transformation Temperature = 10.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature -12.0 °C
10.4 °F
TR10; ASTM D1329
3M Dyneon™ FE 5730 Fluoroelastomer
Composition: Ter-polymer of vinylidene fluoride, hexafluoropropylene and tetrafluoroethyleneLower fluorine version of FE 5830QProcess targets: extrusion onlyProprietary incorporated cure technologyP..
Transformation Temperature -12.0 °C
10.4 °F
TR10; ASTM D1329
3M Dyneon™ FT 2320 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FT 2320 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..