Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 181 - 191 °C | 358 - 376 °F | Temp at Max Expansion |
Akzo Nobel Expancel® 092 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |