Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 95.0 - 100 °C | 203 - 212 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 551 DU 20 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 95.0 - 100 °C | 203 - 212 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 551 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 95.0 - 100 °C | 203 - 212 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 95.0 - 100 °C | 203 - 212 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 551 WU 20 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 95.0 - 100 °C | 203 - 212 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 551 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Transformation Temperature | 95.0 - 100 °C | 203 - 212 °F | Expansion Starting Temperature |
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |