Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature | 730 °C | 1350 °F | Ac<sub>1</sub> |
Carpenter R.D.S.® Alloy Tool Steel (Oil-Hard) (AISI L6) R.D.S. tool steel is an oil hardening die steel which combines extreme toughness with very little size change when heat treated. It is available as a DeCarb-Free product. DCF bars have been cold fin.. |