Transformation Temperature 295 °C
563 °F
Ferro EG 4000 Display Device
Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and ..