Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | -23.0 °C | -9.40 °F | T-10000 Torsional stiffness ASTM D1043-72(1981) |
DuPont Performance Polymers Hypalon® 20 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound
(d Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato.. |