Thermal Properties | Metric | English | Comments |
---|---|---|---|
Clash Berg Stiffness Temperature | -21.0 °C | -5.80 °F | T-10000 Torsional stiffness ASTM D1043-72(1981) |
DuPont Performance Polymers Hypalon® 40S Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(disco Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |
|||
Clash Berg Stiffness Temperature | -21.0 °C | -5.80 °F | T-10000 Torsional stiffness ASTM D1043-72(1981) |
DuPont Performance Polymers Hypalon® 40 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound
(discon Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont .. |