Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 490 °C | 914 °F | ISO 7884-8 |
Schott Glass 8250 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, low refractive index, good insulator X-ray tubes, transmitting tubes, image amplifier tubes, He-Ne-lase.. |
|||
Transformation Temperature, Tg | 490 °C | 914 °F | ISO 7884-8 |
Schott Glass 8270 Borosilicate Glass Borosilicate glass for sealing to Kovar metal and molybdenum, electrically highly insulating, defined UV absorption, stabilized against solarization Backlights The heavy metal content for the elem.. |