Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 449 °C | 840 °F | |
Mo-Sci Corporation WB-40-N White B Filter Glass Applications: Lead-free NVIS White class B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |
|||
Transformation Temperature, Tg | 449 °C | 840 °F | |
Mo-Sci Corporation YB-40-N Yellow B Filter Glass Applications: Lead-free NVIS Yellow class B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |