Polymer Property : Transformation Temperature, Tg = 800 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Transformation Temperature, Tg 800 °C
1470 °F
ISO 7884-8
Schott GM31684 Dental Glass
Remarks: High refractive index glass ceramicApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC..
Transformation Temperature, Tg 800 °C
1470 °F
ISO 7884-8
Schott GM31685 Dental Glass
Remarks: Low refractive index glass ceramicApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCH..