Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 680 °C | 1260 °F | ISO 7884-8 |
Schott 8235 Dental Glass Remarks: Ba-containing, without FApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SCHOTT North .. |
|||
Transformation Temperature, Tg | 680 °C | 1260 °F | ISO 7884-8 |
Schott G018-310 Dental Glass Remarks: Zr-containing, high refractive indexApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by S.. |
|||
Transformation Temperature, Tg | 680 °C | 1260 °F | ISO 7884-8 |
Schott GM32087 Dental Glass Remarks: Sr-containing, low refractive glassApplication: CompositeAdvantagesGreater variety of composition and refractive indiciesOutstanding transparencyBest radiopacitiesInformation Provided by SC.. |