Thermal Properties | Metric | English | Comments |
---|---|---|---|
Transformation Temperature, Tg | 589 °C | 1090 °F | |
Schott N-SF6 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 589 °C | 1090 °F | |
Schott N-SF6HT Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 589 °C | 1090 °F | |
Schott N-LAF35 Glass Information Provided by SCHOTT North America, Inc. |
|||
Transformation Temperature, Tg | 589 °C | 1090 °F | |
Schott RG715 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |