Transformation Temperature, Tg 414 °C
777 °F
Schott SF57 Glass
Information Provided by SCHOTT North America, Inc.
Transformation Temperature, Tg 414 °C
777 °F
Schott SF57HHT Glass
Information Provided by SCHOTT North America, Inc.