Polymer Property : CTE, linear, Parallel to Flow = 25.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 24.0 - 45.0 µm/m-°C

@Temperature 50.0 - 100 °C
13.3 - 25.0 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..