Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
LyondellBasell Lupolen® 4261 A HDPE, Blow Molding Grade Easy-to-process bow molding grade for technical containers such as fuel tanks, petrol filler inlets, expansion tanks, horticultural spray tanks, tanks for lawnmowers, disposable containers (up to 10.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 23.0 - 55.0 °C |
94.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 356 Thermoplastic Polyurethane Desmopan 356 is a TPU on the basis of a standard ester.Applications: Ski boots, castors, shoe heels, technical injection molding parts.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C | 94.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C | 94.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4180 black 9992 PA1010 Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly .. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C | 94.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4180 nat PA1010 Product description: Grilamid XE 4180 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 NATURAL is highly resist.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C | 94.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4181 black PA1010 Product description: Grilamid XE 4181 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 black 9992 is highly .. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C | 94.4 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 4181 nat PA1010 Product description: Grilamid XE 4181 natural is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4181 natural is highly resist.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 55.0 - 160 °C |
94.4 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LT 6040IH Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LT 6040ISH Nylon (Conditioned) ISO data provided by the manufacturer, Arkema. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
Covestro Texin® 255 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |
|||
CTE, linear, Parallel to Flow | 170 µm/m-°C @Temperature 20.0 °C |
94.4 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LT 6040 Flexible Nylon Alloy (Conditioned) Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (500 MPa), good .. |