Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 15.0 - 35.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 19.4 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
CTE, linear, Parallel to Flow | 15.0 - 25.0 µm/m-°C @Temperature 50.0 - 100 °C |
8.33 - 13.9 µin/in-°F @Temperature 122 - 212 °F |
ISO 11359-2 |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
CTE, linear, Parallel to Flow | 15.0 - 20.0 µm/m-°C @Temperature 50.0 - 150 °C |
8.33 - 11.1 µin/in-°F @Temperature 122 - 302 °F |
ISO 11359-2 |
Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
8.33 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® EA 537 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 2410F PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). UL94 V0 and 5VA listing. US FDA and European Food contact approved. Effective June, 2007 this grade will no longer be supported with b.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410R PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature 23.0 - 150 °C |
8.33 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem PW2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-2 |
Solvay Specialty Polymers Ixef® 1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® 1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feature.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-2 |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
8.33 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON EV008 PEI LNP* VERTON* EV008 is a compound based on Polyetherimide containing 40% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5HL black 9914 PA*-GF50 Product description: Grivory GV-5HL black 9914 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-6H EF black 9915 PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50 Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® LVX-50H nat PA12-GF50 Product description: Grilamid LVX-50H natural is a 50% glass fiber reinforced, heat stabilized polyamide 12. Special characteristics of this injection molding product are: Very high stiffness and st.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® XE 3915 PA12-GF50 Product description: Grilamid XE 3915 is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following produce profile:Good UV StabilityHigh impact strengthVe.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BG-50 H PA6-GF50 Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50 Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6.. |
|||
CTE, linear, Parallel to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |