Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® B 1700 000000 PBT PBT, non-reinforced, extrusion, food contact |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® KU 2-7018 000000 PBT PBT, non-reinforced, extrusion, injection molding, impact modified |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Lanxess Pocan® S 1506 901510 PBT PBT, injection molding grade, non-reinforced, elastomer-modified, high impact strength, even at low temperatures |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® 325 PBT (Europe-Africa-Middle East) VALOX 325 is a general purpose, unreinforced PBT injection moulding resin. Applications: sprinklers and nozzles, pumps, doorhandles, tank covers, pens and pencils. |
|||
CTE, linear, Parallel to Flow | 130 - 150 µm/m-°C @Temperature 0.000 - 40.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF) Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
CTE, linear, Parallel to Flow | 130 - 150 µm/m-°C @Temperature 0.000 - 40.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF) Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | |
Solvay Specialty Polymers Solef® 460/461 Polyvinylidene Fluoride (PVDF) Solef® 460/461 PVDF homopolymer has high melt viscosity and is typically processed by extrusion.Features: High Viscosity; HomopolymerAdditional Properties: Crystallization Heat - ASTM D3418 46.0 .. |
|||
CTE, linear, Parallel to Flow | 130 - 180 µm/m-°C @Temperature 0.000 - 40.0 °C |
72.2 - 100 µin/in-°F @Temperature 32.0 - 104 °F |
1 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON MD000I PP (Europe-Africa-Middle East) LNP* Stat-kon* MD000I is a compound based on Polypropylene resin. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 60.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East) VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 80.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® CL500U PBT+PC (Europe-Africa-Middle East) XENOY CL500U is a semi-crystalline blend, developed for exterior automotive parts ( except bumper shells ) and non automotive parts, requiring good impact, excellent chemical resistance and UV stabi.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 0.000 - 100 °C |
72.2 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® FXV310SK PBT VALOX FXV310SK is an unreinforced PBT injection moulding Visualfx* resin with high flow characteristics and containing a metal sparkle. Applications: automotive bezels and appliances. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 26.0 - 200 °C |
72.2 µin/in-°F @Temperature 78.8 - 392 °F |
Mold Direction; ASTM D696 |
Saint-Gobain Fluoroloy® A01 High Performance Seal Material Excellent for light dynamic and static service; Limited wear and heat resistance; Low gas permeability; Good cryogenic properties; Moderate to hard vacuum service; FDA approved.
Information provide.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Load bearing capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in .. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**) Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 20.0 °C |
72.2 µin/in-°F @Temperature 68.0 °F |
|
Covestro Texin® 250 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionCoatingBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScie.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C | 72.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBAFORM C 906 LF POM Copolymer unreinforced, improved wear and friction POMInformation provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
CTE, linear, Parallel to Flow | 130 µm/m-°C @Temperature 23.0 - 55.0 °C |
72.2 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1/-2 |
BASF Ultraform® N2650 Z4 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |