Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 93.6 µm/m-°C | 52.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE TM10 10% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C | 52.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE TM5 5% Talc Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C | 52.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6 TSX10 Nylon 6 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant (10%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C | 52.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® ABS TX15 Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(15%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 93.6 µm/m-°C @Temperature 0.000 - 100 °C |
52.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL EM6101 PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 250F DTUL. Good property retention/wide temperature range. |