Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycolac® X11 ABS Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4501 PPC (Asia Pacific) High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4504 PPC (Asia Pacific) High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® PPC4504 PPC High heat resistant polycarbonate copolymer, provides DTUL of 290F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
51.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 4501 PPC High heat resistant polyphthlate carbonate, provides DTUL of 290F at 264 psi. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C | 51.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR 346 RD Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C | 51.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF15 IM 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites,.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C | 51.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PET GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C | 51.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PA6/6,6 L N Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Copolymer, Fast Molding Cycle, Nucleated and LubricatedProcessing Method: Injection MoldingInformation prov.. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C | 51.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PET GF30 FR X 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 91.8 µm/m-°C @Temperature 20.0 °C |
51.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PlastxWorld CEVIAN® SER91 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |