Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 103 PC (Asia Pacific) Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV stabilized for outdoor and lighting. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 104 PC (Asia Pacific) LEXAN 104 is a high viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information an.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 121R PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 131R PC (Asia Pacific) Nonhalogenated. 3.5 MFR. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 151R PC Lexan 151R resin is a high viscosicty, nonhalogenated resin designed to be a candidate for applications produced via extrusion or blow molding processing.This data was supplied by SABIC-IP for the A.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 203 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 241 PC (Asia Pacific) 10.5 MFR. Improved flame retardance. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 241S PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Super mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 943A PC Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 950 PC Opaque colors, high viscosity, superior flame retardance. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 955A PC (Asia Pacific) Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 955AU PC Lexan* 955AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a V0 UL rating and is UV stabilized, providing additiona.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 144 PC (Asia Pacific) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. Effective January 15th, 2007 this grade is no longer supported with biocompatibility information .. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 925AU PC Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
Techmer ES Elastoblend® PC IM X Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Mold ReleaseFeatures: Impact Modified and Good Mold ReleaseProcessing Method: Injection MoldingInformation provided by TP Compo.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA6/6 C20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and LubricatedAppearance: BlackInf.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron CALIBRE™ 300EP 22 Polycarbonate, General Purpose CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent p.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron CALIBRE™ 891 10 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Styron CALIBRE™ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature 0.000 - 100 °C |
38.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS PPE+PS blend. Unfilled. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature 0.000 - 100 °C |
38.0 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PX1391 PPE+PS (Asia Pacific) Automotive applications, primarily. Excellent electrical properties. high heat. 305F (152C) DTUL. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C | 38.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PC FR UG X GY158 Availability: North AmericaForms: PelletsAdditive: Mold ReleaseFeatures: Flame Retardant and Good Mold ReleaseAppearance: GreyInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 103R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 7.0 MFR, for thicker sections without sinks. UV Stabilized for outdoor and lighting. Internal mold release... |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 940 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. |