Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 905AU PC (Asia Pacific) LEXAN resin grade 905AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in all colors, intended to .. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific) Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Asia Pacific) Lexan LUX9612G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616 PC (Asia Pacific) Lexan LUX9616 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Asia Pacific) Lexan LUX9616G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requirem.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP D1000 PC (Europe-Africa-Middle East) LNP* COLORCOMP* D1000 is a compound based on Polycarbonate resin containing Unfilled Custom Color |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp DBL14 PC (Europe-Africa-Middle East) Internally lubricated Polycarbonate compound, comtaining Glass Bead and PTFEThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® SAN 31 51 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 201-15 Polycarbonate Resin Overview: CALIBREâ„¢ 201-15 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 2061 HD 15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061 HD 15 Polycarbonate Resins are designed for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061 HD 15 Polycarbonate Resins offer a .. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ISO 11359-2 |
Styron CALIBREâ„¢ 2061-15 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-15 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-15 provides excellent heat resistance, impact strength.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 301V-6 Polycarbonate Resin Overview: CALIBREâ„¢ 301V-6 Polycarbonate resins offer exceptional impact resistance and heat distortion resistance, and meets UL94 V-2 rating. CALIBRE 301V-6 contains a mold release agent and is.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
Styron CALIBREâ„¢ 303V-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-10 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products are avai.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate Resin Overview: CALIBREâ„¢ MEGARAD 2081-15 Polycarbonate resin provides end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to hi.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ISO 11359-2 |
Styron CALIBREâ„¢ 302-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 82.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 180 °F |
ASTM D696 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ISO 11359-2 |
Styron CALIBREâ„¢ 302EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C | 37.8 µin/in-°F | ASTM D696 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM D696 |
Styron EMERGEâ„¢ 7700 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7700 Advanced Resin is an ignition-resistant PC/ABS blend that contains no chlorine for bromine additives. It has superior processability for injection molding applicat.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3050 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 68.0 µm/m-°C @Temperature 20.0 °C |
37.8 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 60M10E5 Nylon 6 Alloy, 10% Mineral Filled (Conditioned) RS 60 series rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents). Stability of mechanical, electrical and dimensional properties.Mineral filled.. |