Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E831 |
Polymer Resources PEI-GP1 Polyetherimide, Flame Retardant Polyetherimide, Flame Retardant, High Heat ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL2003 PC Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -40.0 - 95.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000F PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 Listing. Effective June, 2007 this grade will no long.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000P PEI Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010X PEI Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized col.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR 144 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Halogen Free, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR IM HS BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® EH7020 PBT MINERAL FILLED, METALLIZABLE |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
31.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® EH7020 PBT (Asia Pacific) |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® TPU GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Ensinger TECAPEI® made from Ultem® 1000 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 Listing. Effective June, 2007 this grade will no longer.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill FR® PA6/6 FR HS Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized, Halogen Free and LubricatedTPCI# 9857101Information provided by TP Composi.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C @Temperature -20.0 - 150 °C |
31.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June, 2007 this grade will no longer b.. |
|||
CTE, linear, Parallel to Flow | 55.8 µm/m-°C | 31.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA4/6 GF5 HS 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, .. |