Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ Vinyl Rigid Extrusion L6607 Polyvinyl Chloride, Rigid (PVC, Rigid) Physical properties based on Geon L6607 white 1363Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be g.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature 20.0 °C |
27.2 µin/in-°F @Temperature 68.0 °F |
ASTM E381 |
Solvay Specialty Polymers Veradel® A-100, A-200, A-300 Polyethersulfone
(discontinued **) For superior long-term performance at high temperatures in severe service environments. It offers especially good toughness, hydrolytic stability, chemical resistance, plus FDA and USDA compliance.N.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature 23.0 - 100 °C |
27.2 µin/in-°F @Temperature 73.4 - 212 °F |
|
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature -30.0 - 100 °C |
27.2 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 9710 PP SABIC® PPcompound 9710 is a mineral filled, impact modified polypropylene TPO. This material combines high impact resistance, scratch resistance, and heat stability with interior automotive UV st.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3100P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3400P Polyethersulfone (PESU) Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with oth.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU) Veradel® PESU was formerly marketed as Gafone™ PESU. Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They ca.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU) Veradel® A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles.PESU offers excellen.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | |
Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU) Veradel® A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excelle.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP AF004L ABS LNP* THERMOCOMP* AF004L is a compound based on ABS resin containing 20% Glass Fiber. Added feature of this material is: Low Extractible. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
27.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RC008H PA 66 LNP THERMOCOMP* RC008H is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® 3000P Polyethersulfone (PESU)
(Unverified Data**) Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other s.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® A-304P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-304P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C | 27.2 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU)
(Unverified Data**) Veradel A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent t.. |
|||
CTE, linear, Parallel to Flow | 49.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
27.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PFB42EU PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42EU is a compound based on PA 6 resin containing Glass Fiber, Glass Bead. Added features include Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |