Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1285 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1285 PEI (Asia Pacific) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C | 27.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C @Temperature -40.0 - 40.0 °C |
27.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM DU319 PEI Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C | 27.0 µin/in-°F | ASTM D696 |
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information .. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C | 27.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C | 27.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF30 UV 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good UV ResistanceAdditive: UV StabilizerInformation provided by TP Composites.. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C | 27.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 48.6 µm/m-°C | 27.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® HDPE GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |