Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 3.60 - 7.20 µm/m-°C | 2.00 - 4.00 µin/in-°F | |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
CTE, linear, Parallel to Flow | 3.60 - 7.20 µm/m-°C | 2.00 - 4.00 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP)
(Unverified Data**) Xydar G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology. The moldabili.. |