Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, DRY Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -30.0 - 100 °C |
17.8 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 8620A PP SABIC® PPcompound 8620A is a mineral filled, impact modified polypropylene TPO. It was originally designed for painted automotive bumper fascia applications where a combination of good flow, hig.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp RFN16SXS PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN16SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Euro.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12 LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
17.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DF006HL PC LNP THERMOCOMP* DF006HL is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Low Extractible, Healthcare. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66 LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 LNP* THERMOCOMP* RF-1008 is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP WF006 PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* WF006 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP ZFM3314 PPE (Europe-Africa-Middle East) glas, mineral filled PPE |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF MF0049I PP (Europe-Africa-Middle East) LNP* THERMOTUF* MF0049I is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features include; Flame Retardant, Chemically Coupled. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C | 17.8 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 9405H-1 Glass Filled Electrical Encapsulation Grade Epoxy E-9504H-1 is glass fiber filled epoxy molding compound designed for encapsulation of delicate electrical components as well as large coils. Excellent thermal shock, moldability, and retention of ele.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
17.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF008XXH PA 66 LNP* THERMOCOMP* RF008XXH is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added feature of this material includes: Healthcare. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C | 17.8 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-KG6 PA410-GF30 % Glass Reinforced, Heat Stabilized, for E&E applications |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 20.0 - 93.3 °C |
17.8 µin/in-°F @Temperature 68.0 - 200 °F |
Parallel to Laminate |
CIP Composites 200 Series Laminated Polymer Bearing Material The 200 series consists of PTFE/polyester combination fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated ma.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C | 17.8 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-HG6 PA410-GF30 30% Glass Reinforced, Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 20.0 - 93.3 °C |
17.8 µin/in-°F @Temperature 68.0 - 200 °F |
Parallel to Laminate |
CIP Composites 100 Series Laminated Polymer Bearing Material The 100 series consists of polyester fabric and one of several solid lubricants (optional) in a resin matrix. Non-metallic, high load, high impact and self lubricating laminated material. Laminated.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam BFR330A PA6, Glass Bead Reinforced, Flame Retardant, Injection Molded Starflam BFR330A is a Flame Retardant, Glass Bead Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C | 17.8 µin/in-°F | ISO 11359 |
BASF Petra® 110 BK-112 15% Glass Filled PET Petra 110 is a 15% glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a good combination of performance properties including good strength a.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C | 17.8 µin/in-°F | ISO 11359 |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 20.0 °C |
17.8 µin/in-°F @Temperature 68.0 °F |
ISO data |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Dry)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East) LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber |
|||
CTE, linear, Parallel to Flow | 32.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
17.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East) LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified. |