Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ASTM D696 |
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ASTM D696 |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFL146 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFL146 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
|
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66 LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RFL449 PA 66 LNP* LUBRICOMP* RFL449 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 20% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP SCL36 PA12 LNP* LUBRICOMP* SCL36 is a compound based on Nylon 12 resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WFL369 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WFL369 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE. Added features include: Flame Retardant, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON RX98063 PA 66 (Europe-Africa-Middle East) LNP* STAT-KON* RX98063 is a compound based on PA 66 resin containing Glass Fiber, Stainless Steel Fiber. Added features include; Antistatic. |
|||
CTE, linear, Parallel to Flow | 28.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC LNP* Thermocomp* DF004RXP is a compound based on Polycarbonate resin containing 20% Glass Fiber. Some light color grades may have lower impact data than natural and black. Added features include: .. |
|||
CTE, linear, Parallel to Flow | 28.9 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DF004RXP PC (Asia Pacific) 20% Glass Fiber Reinforced Polycarbonate. Some light color grades may have lower impact data than nature and black grade. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PFB55 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB55 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber |
|||
CTE, linear, Parallel to Flow | 28.9 µm/m-°C @Temperature -40.0 - 40.0 °C |
16.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GFN2 PPE+PS PPE+PS blend. 20% Glass reinforced. UL746C F1. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional sta.. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON FX91304 PE LNP* STAT-KON* FX91304 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
16.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m.. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
16.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 20.0 °C |
16.1 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® KL 1-1427 Polycarbonate/ABS Blend Glass fiber reinforced grade (30%) with high stiffness.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – .. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 20.0 °C |
16.1 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C @Temperature 20.0 °C |
16.1 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America RX® 1-510N Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
CTE, linear, Parallel to Flow | 29.0 µm/m-°C | 16.1 µin/in-°F | ISO 11359-2 |
Solvay Specialty Polymers Ixef® 5002 Polyarylamide (PARA), 20% GlassPTFE
(discontinued **) Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.- Natural: Ixef 5002/008.. |