Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM D696 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DFP36 PC (Europe-Africa-Middle East) LNP* Lubricomp* DFP36 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Silicone. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 85.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 185 °F |
ISO 11359 |
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL36 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RX05049 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Proprietary Lubricant. Added features include; Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP UX06427 PPA LNP* LUBRICOMP* UX06427 is a compound based on PPA containing 30% Carbon Fiber, 15% PTFE. Added features of this grade include: Heat Stabilized, Hot Water Moldable, Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DE003Z PC LNP STAT-KON* DE003Z is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Extrusion Grade. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP IF00C PA6.12 LNP* THERMOCOMP* IF00C is a compound based on Nylon 6/12 resin containing 60% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
12.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OF008E PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OF008E is a compound based on PPS - Linear resin containing Glass Fiber. Added features include: Easy Molding. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ASTM E831 |
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
ASTM E-831 |
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
12.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WCP36 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WCP36 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber, PTFE, Silicone. Added features include; Internally Lubricated, Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature 20.0 °C |
12.2 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP UX08325 PPA (Asia Pacific) LNP* Thermocomp* UX08325 is PPA base glass fiber filled compounds, good for LDS (Laser direct structuring)application. Additional feature is high heat. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® 940 BK505 Polyethylene Terephthalate (PET)
(Unverified Data**) 40% Glass/Mineral Reinforced Polyethylene Terephthalate Rynite 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength stiffness and low warpage.Informatio.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G30HSL NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATRON C2040G5 PPS, cross-linked, 40% GF, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | ISO 11359-1/-2 |
Barlog Plastics KEBATRON L2040G3 PPS, linear, 40% glass fiber reinforced, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C | 12.2 µin/in-°F | TMA |
Vyncolit W5020 Glass Filled Novolac Phenolic Novolac resin based, glass fiber and glass bead reinforced. High dimensional stability and excellent chemical resistance at high temperatures in hydraulic brake fluids. Used in the ABS system.Inform.. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Verton UX06451 BK8-312 PPA LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East) LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |
|||
CTE, linear, Parallel to Flow | 22.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
12.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP VERTON UX06451 BK8-312 PPA (Asia Pacific) LNP* Verton* UX06451 BK8-312 is a compound based on Polyphthalamide resin containing Long Glass Fiber. |