Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 0.594 µm/m-°C @Temperature -30.0 - 100 °C |
0.330 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM E831 |
ExxonMobil Exxtral™ H1025 Performance Polyolefin Product Description: A specialty thermoplastic olefin resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for automotive exterior applications.Availability.. |