Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 90.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2863 C Colored ASA+PC
Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
CTE, linear, Parallel to Flow 70.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2864 C Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
CTE, linear, Parallel to Flow 70.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2864 C UV Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
CTE, linear, Parallel to Flow 50.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
27.8 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
CTE, linear, Parallel to Flow 80.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
44.4 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
BASF Ultradur® B 4300 K4 20% Glass Bead Filled PBT
Description: Is a PBT + ASA, Injection-molding grades containing 20% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit..
CTE, linear, Parallel to Flow 70.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2861/1 C Colored ASA+PC
Description: Grade with high heat resistance for injection molding and extrusion.Applications: Interior and exterior automotive parts, and electrical housings.Information provided by STYROLUTION, wh..
CTE, linear, Parallel to Flow 70.0 - 90.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 - 50.0 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/-2
Styrolution Luran® S KR 2863 C UV Colored ASA+PC
Description: Grade with very high heat resistance for automotive interiors and exteriors as well as electrical parts.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Copyright © lookpolymers.com All Rights Reserved