Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 50.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 BK 23213 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 60.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
CTE, linear, Parallel to Flow | 60.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
33.3 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4350 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
CTE, linear, Parallel to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
CTE, linear, Parallel to Flow | 50.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 BK60564 30% Mineral Filled PA6 (Dry) ultramid B3M6 BK60564 is a 30% mineral reinforced, pigmented black injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent lase.. |
|||
CTE, linear, Parallel to Flow | 50.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
27.8 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry) Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF |
|||
CTE, linear, Parallel to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl FN215D PPE+HIPS (Europe-Africa-Middle East) NORYL FN215 is a Noryl Engineering structural foam grade fulfilling a wide range of application requirement. Moulded with the recommended blowing agents, this material provides all the performance r.. |