Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature 20.0 °C |
51.7 µin/in-°F @Temperature 68.0 °F |
|
Eastman Tenite 383A-10 Cellulose Acetate Propionate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
51.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
51.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP KB008 Acetal Copolymer LNP THERMOCOMP* KB008 is a compound based on Acetal Copolymer resin containing 40% Glass Bead. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
51.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide BST42 PA6, Impact Modified, Injection Molded BST42 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature 20.0 °C |
51.7 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C | 51.7 µin/in-°F | ISO 11359 |
BASF Ultramid® 8254 HS BK-102 PA6 (Dry) Ultramid 8254 HS is a highly flexible, heat stabilized, impact modified nylon 6 extrusion grade for tubing applications. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature 20.0 °C |
51.7 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 6000CD Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
CTE, linear, Parallel to Flow | 93.0 µm/m-°C @Temperature 20.0 °C |
51.7 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® RS 6000TLA Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |