Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Americas Styrenics Styron® 484C High Impact Polystyrene
(discontinued **) STYRON® 484C high impact polystyrene resin, is typically used in refrigeration applications, appliances, containers, lids, furniture and profiles. It offers excellent low temperature toughness, exc.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics GELOY CR7020 ASA (Europe-Africa-Middle East) GELOY CR7020 is a profile extrusion and co-extrusion grade, blend of ASA/SAN. In co-extrusion it can be used over CYCOLAC, PVC or other compatible polymers. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® QE 1120, Extrusion Grade
(discontinued **) General purpose extrusion grade.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with .. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS NOVODUR® P2L-AT ABS, Injection Grade
(discontinued **) Injection molding grade, very easy flow, antistatic, high stiffness, high gloss.Applications: Telephones, household goods, disk and video housings, office equipment.Information provided by the manuf.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL C333/m² ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-20 Special low gloss grade for injection moulding which combines medium heat resistance with a good b.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL PD H210/K ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,085-25-16-25 Flame retarded (PBBE free) injection moulding grade, rated UL94-5V at 3.2 mm thick and UL 94V-0 at.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® F223-DH (Dry) Low/Medium Viscosity, Heat Stabilized Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® 488 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Noryl V190 PPE+HIPS (Europe-Africa-Middle East) NORYL V190 is an unfilled flame retardant material with a Vicat B/120 of 90°C according ISO 306. NORYL V190 is V1 at 2.0 mm according UL94 and halogen free according VDE/DIN 472 part 815.This dat.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359 |
Styrolution Terblend® N NM-12 ABS/PA6 (Dry) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359 |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX902E PPE+PA (Europe-Africa-Middle East) NORYL GTX902E is a low cost GTX grade especially developed for automotive (wheel)trims. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
50.0 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East) NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT6000 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedinjection molding grade Makroblend DP UT6000* offers an exceptional low-temperature impact strength, good flowability and excellent chemical resis.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT6003 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedUV-stabilizedinjection molding grade Makroblend DP UT6003* offers an exceptional low-temperature impact strength, good flowability and excellent c.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
50.0 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C | 50.0 µin/in-°F | ISO 11359-1/-2 |
DSM Arnite® T06 202 /A PBT Medium Viscosity, Injection Molding |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® 452
(discontinued **) Key Features:UnfilledSuitable processing methods:Sheet extrusionThermoformingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after I.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL D160 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-08-09-25 Very high heat injection moulding grade with good flow. Permits production of complex, thin walled.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ASTM data |
Americas Styrenics Styron® 425 High Impact Polystyrene
(discontinued **) STYRON® 425 impact polystyrene resin is typically used in thin section parts, hot drink cups and cassettes. It offers heat resistance, easy flow, fast cycling, and excellent tensile and flex proper.. |
|||
CTE, linear, Parallel to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
|
Polimeri Europa SINKRAL L320 ABS